Fatigue Characteristic of Designed T-Type Specimen under Two-Step Repeating Variable Amplitude Load with Low-Amplitude Load below the Fatigue Limit

Jin Gan    
Di Sun    
Hui Deng    
Zhou Wang    
Xiaoli Wang    
Li Yao and Weiguo Wu    

Resumen

In order to investigate the non-linear fatigue cumulative damage of joints in ocean structural parts, one type of low carbon steel Q345D was employed to prepare designed T-type specimens, and a series of fatigue experiments were carried out on the specimens under two-step repeating variable amplitude loading condition. The chosen high cyclic loads were larger than the constant amplitude fatigue limit (CAFL) and the chosen low cyclic loads were below the CAFL. Firstly, the S-N curve of designed T-type specimen was obtained via different constant amplitude fatigue tests. Then, a series of two-step repeating variable load were carried out on designed T-type specimens with the aim of calculating the cumulative damage of specimen under the variable fatigue load. The discussions about non-linear fatigue cumulative damage of designed T-type specimens and the interaction effect between the high and low amplitude loadings on the fatigue life were carried out, and some meaningful conclusions were obtained according to the series of fatigue tests. The results show that fatigue cumulative damage of designed T-type specimens calculated based on Miner?s rule ranges from 0.513 to 1.756. Under the same cycle ratio, the cumulative damage increases with the increase of high cyclic stress, and at the same stress ratio, the cumulative damage increases linearly with the increase of cycle ratio. Based on the non-linear damage evaluation method, it is found that the load interaction effect between high and low stress loads exhibits different damage or strengthening effects with the change of stress ratio and cycle ratio.